Clarification on the stress corrosion phenomenon detected on parts of the auxiliary circuits of the main primary circuit of several nuclear reactors

Clarification on the stress corrosion phenomenon detected on parts of the auxiliary circuits of the main primary circuit of several nuclear reactors On 10 March 2023, EDF proposed to the ASN (Nuclear safety authority) an evolution in its stress corrosion control strategy. EDF is accelerating the inspection of the concerned welds of the RIS and RRA systems, in order to include the elements identified on the weld repaired at Penly 1 1.The ASN announced today to have taken note of...
Comunicato Precedente

next
Comunicato Successivo

next

Clarification on the stress corrosion phenomenon detected on parts of the auxiliary circuits of the main primary circuit of several nuclear reactors

On 10 March 2023, EDF proposed to the ASN (Nuclear safety authority) an evolution in its stress corrosion control strategy. EDF is accelerating the inspection of the concerned welds of the RIS and RRA systems, in order to include the elements identified on the weld repaired at Penly 11.

The ASN announced today to have taken note of this evolution in the strategy, and to continue the technical dialogue with EDF to ensure the relevance of the planned schedule2.

To date and on the basis of the control strategy proposed by EDF, the estimate of nuclear output in France for 2023 remains in the range 300-330TWh.

This press release is certified. Check its authenticity on medias.edf.com

About EDF
As a major player in energy transition, the EDF Group is an integrated energy company active in all businesses: generation, transmission, distribution, energy trading, energy sales and energy services. EDF group is a world leader in low-carbon energy, having developed a diverse production mix based mainly on nuclear and renewable energy (including hydropower). It is also investing in new technologies to support energy transition. EDF's raison d'être is to build a net zero energy future with electricity and innovative solutions and services, to help save the planet and drive well-being and economic development. The Group is involved in supplying energy and services to approximately 40.3 million customers (1), of whom 30.3 million in France (2). It generated consolidated sales of €143.5 billion in 2021. EDF is listed on the Paris Stock Exchange.

(1) Since 2018, customers are counted per delivery site. A customer can have two delivery points: one for electricity and another one for gas.
(2) Including ÉS (Électricité de Strasbourg) and SEI.


1 See information note of 8 March 2023: https://www.edf.fr/sites/groupe/files/2023-03/EDF Stress Corrosion_SSE_030622.pdf
2 See press release of the ASN of 16 March 2023

Attachment

  • PR_Update corrosion

Per maggiori informazioni
Sito Web
edf-re.com

Ufficio Stampa

 Nasdaq GlobeNewswire (Leggi tutti i comunicati)
2321 Rosecrans Avenue. Suite 2200
90245 El Segundo Stati Uniti

Allegati
Slide ShowSlide Show
Non disponibili
;